AO & EO Crystal |
Ф4//SAW grade LN Tc=1142±3℃ THs:0.35,0.5, TTV 10μm, BOW 20μm |
|
Ф4//SAW grade LT Tc=605±3℃ THs:0.35, TTV 10μm, BOW 20μm |
|
Ф3//optical grade LN Fe,Cu,Ni,Cr<1ppm Tc=1142±1℃ Transmission >70% @ 632.8nm homogeneity:<5×10-5/cm |
|
Doped Fe:LN Doped Zn:Fe:LN Doped MgO:LN |
|
LN optical wave guide wafer Parallelism <20" Wave front distortion <λ/4 |
|
Electr-optical switch Extinction rate >200:1 Optical damage threshold:≥100MW/cm2 @1064nm |
|
3inch PPLN wafer MgO:PPLN wafer Transmit thickness:0.5,0.8mm period:5~30μm |